Product Details:
Payment & Shipping Terms:
|
Elongation At Break (%): | 7.0-8.5 | Diameter(mm): | 0.89-0.92 |
---|---|---|---|
Application: | Automobiles, Bicycle, Bike, Motorcycles, Planes, Vehicles | Feature: | Bronze Coated, Durable, Rustproof, Waterproof |
Break Force (N): | 2100-2260 | Yield Rate (%): | 93.3-94.9 |
High Light: | annealed wire,high tensile steel wire,coated steel wire |
2260N Break Force Annealed Steel Wire For Car Tire , Φ 0.9MM
Description:
Bead wire for tire rim is widely applied to the manufacturing of various tires rims for automobiles,motorcycles,planes as well as other vehicles.It’s the pivotal material of tire,which can strengthen the tire and is considered an important raw material for the tyre manufacturing business.
Specifications:
Description |
BEAD WIRE |
Reference |
GB/T14450- 2008 |
Diameter |
Φ0.9mmHT |
||||
Item |
Standard |
Result |
|||||||
Diameter(mm) |
0.9±0.02 |
0.89-0.92 |
|||||||
Break force (N) |
≥2100 |
2100-2260 |
|||||||
Yield rate (%) |
93.0-96.0 |
93.3-94.9 |
|||||||
Elongation at break(%) |
≥5.0 |
7.0-8.5 |
|||||||
Torsion(360°/200d) |
≥50 |
59-75 |
|||||||
Residual torsion (° /9m) |
≯360 |
90-120 |
|||||||
Bronze coated(g/kg) |
0.35-0.65 |
0.40-0.51 |
|||||||
Sn (%) |
0.5-3.0 |
0.7-1.5 |
|||||||
Straightness (mm/3m) |
≤500 |
180-460 |
|||||||
Adhesion (N/50mm) |
≥1200 |
1242 |
|||||||
Surface Quality |
Coating Smooth and uniform |
conform |
|||||||
Assay of chemical contents |
|||||||||
C |
Mn |
Si |
P |
S |
|||||
0.70-0.72 |
0.50-0.60 |
0.17-0.26 |
0.006-0.016 |
0.005-0.018 |
Competitive advantage: